Wst. 1.4876/1.4958/1.4959
UNS N08800/N08810/N08811
Lagerprogramm: Auf Anfrage
Spezifikationen: ASTM B 407 / ASTM B 163 / ASME SB-163 / EN ISO 1127/96/NACE MR0175
Maximale Betriebstemperatur: 1100°C/2000°F
Chemische Zusammensetzung (%) | Cr | Ni | Mn | Cu | Si | C | S | Ti | Al | Bal. | |||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
800 | min | 19.0 | 30.0 | – | – | – | – | – | 0.15 | 0.15 | 39.5 | ||||||||||
max | 23.0 | 35.0 | 1.50 | 0.75 | 1.0 | 0.100 | 0.015 | 0.60 | 0.60 | – | |||||||||||
800H | min | 19.0 | 30.0 | – | – | – | 0.050 | – | 0.25 | 0.25 | 39.5 | ||||||||||
max | 23.0 | 35.0 | 1.50 | 0.75 | 1.0 | 0.100 | 0.015 | 0.60 | 0.60 | – | |||||||||||
800HT | min | 19.0 | 30.0 | – | – | – | 0.060 | – | 0.25 | 0.25 | 39.5 | ||||||||||
max | 23.0 | 35.0 | 1.50 | 0.75 | 1.0 | 0.100 | 0.015 | 0.60 | 0.60 | – |
Mechanische Eigenschaften | 800 | 800H | 800HT | |||
---|---|---|---|---|---|---|
Festigkeit (mpa, min) | 536 | 448 | 448 | |||
Streckgrenze (0.2% offset mpa, min) | 150 | 172 | 172 | |||
Dehnung (%, min) | 20 | 20 | 20 | |||
Dichte / Gewicht (g / cm3 / kg) | 7.94 | 7.94 | 7.94 |